MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Lehvoss LUVOCOMĀ® 1301-7815 Polyphenylene sulfide, Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler

Material Notes: Polyphenylene sulfide, linear with carbon fibers, lubricant modified, grey

Main features: Improved friction and wear behavior, self-lubricating, for highest tribological requirements. High-strength and stiffness parts with low creep. Electrically conductive, suitable for continuous discharging of statically-generated electricity. High continuous use and heat-distortion temperatures. Non flammable.

Information provided by Lehmann & Voss & Co.KG

Vendors:
Available Properties
  • Specific Gravity, ISO 1183-3
  • Water Absorption, ISO 62
  • Linear Mold Shrinkage, DIN 16742
  • Melt Flow
  • Tensile Strength, ISO 527, 50 mm/min
  • Elongation at Break, ISO 527, 50 mm/min, Fmax
  • Tensile Modulus, ISO 527, 1 mm/min
  • Flexural Strength, ISO 178, 10 mm/min
  • Flexural Modulus, ISO 178, 2 mm/min
  • Flexural Strain at Break, ISO 178, 10 mm/min, Fmax
  • Charpy Impact Unnotched, ISO 179 1eU, 80x10x4mm
  • Coefficient of Friction, ASTM G137, 100Cr6, 13 m/s; Block on Ring
  • K (wear) Factor, ASTM G137, Sp. Wear Rate-Block on Ring, vs. 100Cr6, 1 m/s
  • K (wear) Factor, ASTM G137, Sp. Wear Rate-Block on Ring, vs. 100Cr6, 1 m/s
  • Surface Resistance, DIN EN 62631-3-2, Ronde 60x4mm
  • Insulation Resistance, DIN EN 62631-3-3, strip electrode R25
  • Maximum Service Temperature, Air, IEC 60216, Continuous
  • Maximum Service Temperature, Air, during lifetime
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75, 80x10x4mm
  • Nozzle Temperature
  • Zone 1
  • Zone 2
  • Zone 3
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature, Dehumidifying
  • Drying Temperature, Dehumidifying
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Lehvoss; Lehmann & Voss & Co.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.