| MAGNIFIN H-5 A is a high-purity magnesium hydroxide surface treated with a special vinyl silane coating. Based on a mineral raw material, the patented process guarantees a regular structure of the crystallite. MAGNIFIN H-5 A is tailor-made for plastic and elastomer applications, e.g. XLPE, XL-EVA, EPDM, and EPM, and represents a halogen free flame retardant with low smoke emission and high thermal stability up to 340°C. During the decomposition process no toxic or corrosive gases are generated. The surface treatment favors the compatibility of filler and polymer matrix and therefore improves the mechanical properties of the compound CAS No.: 1309-42-8 EC/EINECS No.: 215-170-3 Information provided by J.M. Huber Corporation |