MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Kennametal Stellite Stellite® 33
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Completely non-magnetic. Specific Electrical Resistance: 39.8 µOhm/in^3.

Applications: standard tool bits, tipped tools, form tools, milling cutter blades, wood working tools, reamer blades, cut-off tools, valves, valve seats, hot extrusion dies, plug gages, indicator anvils, wire guides, wear strips, balls, glass shear blades, nozzles and hot forming dies.

Corrosion: Resists corrosion by moist atmosphere, salt spray, milder acids, and certain strong acids. Excellent resistance to lead oxide corrosion, losing 0.18-0.20 grams per square inch per hour at 927°C.

Machinability: Generally finished by grinding, should be well honed, using a hand hone to remove any grinding burr.

Weldability: Cannot be welded by fusion or pressure methods. Most satisfactorily joined to steel by brazing silver solder and a paste flux are recommended.

Data provided by the manufacturer, Deloro Stellite, Inc.

Product of former Deloro Stellite Inc.

Vendors:
Available Properties
  • Density
  • Hardness, Rockwell C, average
  • Tensile Strength, Ultimate
  • Modulus of Elasticity
  • Magnetic Permeability, at 200 Oersted
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co, As remainder
  • Iron, Fe
  • Silicon, Si
  • Tungsten, W
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Kennametal Stellite, former Deloro Stellite Inc

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.