MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Trinseo CALIBRE™ MEGARAD™ 2081-6LR Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Gamma Radiation Resistant

Material Notes: CALIBRE™ MEGARAD 2081-6LR Polycarbonate resin was developed for medical applications requiring improved resistance to lipids over standard polycarbonate resin. When exposed to a 20% intralipid emulsion solution under strained conditions, CALIBRE™ MEGARAD 2081-6LR exhibits significant property retention compared to standard polycarbonate. It also provides end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (gamma or electron beam). CALIBRE™ MEGARAD 2081-6LR can reduce the color shift by 50% compared to general purpose polycarbonate resins.

Main Characteristics:

  • Improved lipid resistance
  • Stabilized for high-energy radiation
  • Tested under ISO 10993
  • Transparent
  • Contains mold release
Applications:
  • Medical applications

Information provided by Trinseo.

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ISO 62
  • Moisture Absorption at Equilibrium, ISO 62, 50% RH
  • Linear Mold Shrinkage, Flow, ASTM D955
  • Melt Flow, ASTM D1238
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength at Break, ASTM D638, 50 mm/min
  • Tensile Strength, Yield, ASTM D638, 50 mm/min
  • Elongation at Break, ASTM D638, 50 mm/min
  • Elongation at Yield, ASTM D638, 50 mm/min
  • Tensile Modulus, ASTM D638, 50 mm/min
  • Flexural Strength, ASTM D790, Method I (3 point load), 2.0 mm/min
  • Flexural Modulus, ASTM D790, Method I (3 point load), 2.0 mm/min
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D256
  • Tensile Impact Strength, ASTM D1822
  • Dart Drop, Total Energy, ASTM D3763, 3.39 m/sec
  • Abrasion, ASTM D1044, [%], Taber
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • CTE, linear, Parallel to Flow, ASTM D696
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Annealed
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Unannealed
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Annealed
  • Vicat Softening Point, ASTM D1525
  • Refractive Index, ASTM D542
  • Haze, ASTM D1003
  • Transmission, Visible, ASTM D1003
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Trinseo, former Styron

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

USP Class VI adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.