| Emulprene 1502CR is a Styrene-Butadiene copolymer, cold polymerized using fatty acid as emulsifier, coagulated with salt-acid and stabilized with a non-staining antioxidant. Between 4 and 12 % of calcium carbonate is used as dusting agent. Uses: Emulprene 1502CR is widely used like raw material in tires, heels, shoe soles and for the production of transparent goods, and light colors and adhesives. Information provided by Dynasol Group. |