| Molecular Formula: C14H15O2NS Properties : It is white or yellow crystalline. It can be dissolved in acetone, benzene, toluene, ethyl ether and ethyl acetate as well as warm carbon tetra chloride, ethyl alcohol and heptane. It also can be slightly dissolved in gasoline, but not in kerosene and water. Application : The product may be used in natural rubber and synthetic rubber. It may protect effectively the rubber material from scorching during Processing, So that to make it possible for extruder and calendar to be running at a high temperature and high speed and improve the production capacity of vulcanizer. The product also can improve the storage stabilization of the rubber material, protect natural vulcanization during storage. It has reclaimation function for rubber material, which bearing high heating or with dangers of scorching. Information provided by Ganpati Exim PVT. LTD. |