| Stability: Stable under recommended storage conditions. Molecular Formula: [CH2CH(CH2NH2)]n free base Synonyms: POLY(ALLYLAMINE);POLYALLYLAMINE 05L;2-Propen-1-amine,homopolymer;Poly(allylamine) solution;POLY(ALLYLAMINE), 20 WT. % SOLUTION IN W ATER, AVERAGE MW CA. 65,000;POLY(ALLYLAMINE), 20 WT. % SOLUTION IN W ATER, AVERAGE MW CA. 17,000;2-Propenamine homopolymer; Alfa Chemistry Materials product group: Polymer/Macromolecule Manufacturer data sheet |