MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Solvay FM® 400NA Epoxy Film Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: FM® 400NA adhesive film is the non-asbestos version of FM 400 and is designed to provide similar performance to that of FM 400 adhesive across the board. It is supplied with a lightweight nylon carrier and is designed for bonding metal-to-metal and sandwich composite structures requiring long time exposures to 420°F (216°C). BR® 400 is a modified epoxy corrosion inhibiting primer and provides excellent corrosive resistance when used on aluminum structures. FM 400NA adhesive film will also bond to BR® 127 primer with normal results. Where corrosion resistance is not required, FM 400NA adhesive film can be used without primer. FM 400NA adhesive film can be cured over a wide range of heat-up rates, temperatures and pressures. The recommended cure cycle is a 3 to 8.5°F/min (1.6 to 4.7°C/min) heat-up rate with a 60 minute hold at 350 ± 10°F (177 ± 5.6°C) and 45 ± 10 psi (0.31 ± 0.07 MPa) pressure.

Features & Benefits:

  • Designed to bond metal-to-metal and honeycomb sandwich structures
  • Long term thermal resistance at 420°F (216°C)
  • Structural performance from -67 to Note 1: FM 400NA film with BR 400 primer, 2024-T81 bare aluminum substrates 420°F (-55 to 216°C)
  • Does not contain asbestos
  • Can be cured with a wide range of heat-up rates
Applications:
  • Honeycomb sandwich construction
  • Metal-to-metal bonding
Note 1: FM 400NA film with BR 400 primer, 2024-T81 bare aluminum substrates

Note 2: FM 400NA film with BR 400 primer, 0.050 in. (1.27 mm) Ti6-4V annealed titanium substrates

Information provided by Cytec, subsequently acquired by Solvay.

Vendors:
Available Properties
  • Volatiles
  • Storage Temperature
  • Tensile Strength, Flatwise, Aged 3 hours at 420°F (216°C) - Tested at 420°F (216°C)
  • Tensile Strength, Flatwise, Aged 18 hours at 365°F (185°C) - Tested at 365 ± 5°F (185 ± 3°C)
  • Tensile Strength, Flatwise, 75 ± 5°F (24 ± 3°C)
  • Flexural Strength, Aged 3 hours at 420°F (216°C) - Tested at 420°F (216°C)
  • Flexural Strength, Aged 18 hours at 365°F (185°C) - Tested at 365 ± 5°F (185 ± 3°C)
  • Flexural Strength, 75 ± 5°F (24 ± 3°C)
  • Shear Strength, Note 1, 10 min at 420 ± 5°F (216 ± 3°C)
  • Shear Strength, Note 1, Aged 3 hours at 420°F (216°C)- Tested at 420°F (216°C)
  • Shear Strength, Note 1, 10 min at 365 ± 5°F (185 ± 3°C)
  • Shear Strength, Note 2, Aged 3 hours at 420°F (216°C) - Tested at 420°F (216°C)
  • Shear Strength, Note 1, Aged 18 hours at 365°F (185°C)- Tested at 365 ± 5°F (185 ± 3°C)
  • Shear Strength, Note 2, Aged 18 hours at 365°F (185°C) - Tested at 365 ± 5°F (185 ± 3°C)
  • Shear Strength, Note 1, 7 days immersion at 75°F (24°C) in MIL-A-8243
  • Shear Strength, Note 1, 7 days immersion at 120°F (49°C) in MIL-T-5624
  • Shear Strength, Note 1, 7 days immersion at 75°F (24°C) in hydraulic fluid (MIL-H-5606)
  • Shear Strength, Note 1, 10 min at 75 ± 5°F (24 ± 3°C)
  • Shear Strength, Note 1, Aged 18 hours at 365°F (185°C)- Tested at 75 ± 5°F (24 ± 3°C)
  • Shear Strength, Note 1, 10 min at -67 ± 5°F (-55 ± 3°C)
  • Shear Strength, Note 1, 7 days immersion at 120°F (50°C) in hydrocarbon fluid (TT-S-735, Type I)
  • Shear Strength, Note 2, 10 min at 75 ± 5°F (24 ± 3°C)
  • Shear Strength, Note 2, Aged 18 hours at 365°F (185°C) - Tested at 75 ± 5°F (24 ± 3°C)
  • Shear Strength, Note 2, 10 min at -67 ± 5°F (-55 ± 3°C)
  • Peel Strength, Bell Metal-to-Metal, At 75 ± 5°F (24 ± 3°C)
  • Peel Strength, Bell Metal-to-Metal, 10 min. at -67 ± 5°F (-55 ± 3°C)
  • Maximum Service Temperature, Air, long term
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.