MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
3M 5200 Marine Adhesive/Sealant
Categories: Polymer; Adhesive

Material Notes: 3M™ Marine Adhesive/Sealant 5200 is a one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds. It has excellent adhesion to wood, gelcoat and fiberglass. It forms a watertight, weather-resistant seal on joints and boat hardware, above and below the waterline. In addition, its flexibility allows for dissipation of stress caused by shock, vibration, swelling or shrinking

Features:

  • Tough/flexible polyurethane polymer
  • Non-shrinking
  • One-part moisture cure
  • Long working time

Information provided by 3M

Vendors:
Available Properties
  • Density
  • Solids Content
  • Hardness, Shore A, cured
  • Tensile Strength at Break, Salt Water
  • Tensile Strength at Break, Fresh Water
  • Tensile Strength at Break, 50% RH
  • Elongation at Break, Salt Water
  • Elongation at Break, 50% RH
  • Elongation at Break, Fresh Water
  • Shear Strength, Overlap, Polyethylene, 50% RH
  • Shear Strength, Overlap, Polypropylene, 50% RH
  • Shear Strength, Overlap, Lead, 50% RH
  • Shear Strength, Overlap, Nylon, 50% RH
  • Shear Strength, Overlap, Copper, 50% RH
  • Shear Strength, Overlap, Acrylic, 50% RH
  • Shear Strength, Overlap, ABS, 50% RH
  • Shear Strength, Overlap, Bronze, 50% RH
  • Shear Strength, Overlap, Stainless Steel, 50% RH
  • Shear Strength, Overlap, Fiberglass, 50% RH
  • Shear Strength, Overlap, Polycarbonate, 50% RH
  • Shear Strength, Overlap, Aluminum, 50% RH
  • Shear Strength, Overlap, Brass, 50% RH
  • Shear Strength, Overlap, Zinc (Galvanized), 50% RH
  • Shear Strength, Overlap, Teak, 50% RH
  • Shear Strength, Overlap, Gelcoat, 50% RH
  • Shear Strength, Overlap, Steel, 50% RH
  • Shear Strength, Overlap, Oak, 50% RH
  • Shear Strength, Overlap, Mahogany, 50% RH
  • Shear Strength, Overlap, Maple, 50% RH
  • Shear Strength, Overlap, Pine, 50% RH
  • Shear Strength, Overlap, Fir, 50% RH
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, Full Cure, 50% RH
  • Working Life, Open Time, 90% RH
  • Working Life, Open Time, 50% RH
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.