MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Phillips 66 Syncon® ISO Grade 46 Turbine Oil
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Syncon Turbine Oil is a premium quality, synthetic lubricant developed for use in land-based gas turbines operating over a wide temperature range, where the manufacturer calls for a synthesized hydrocarbon (SHC) or PAO-based turbine oil. Syncon Turbine Oil is formulated with synthetic polyalphaolefin (PAO) base oils and select additives to provide outstanding performance and protection in gas turbines. It has outstanding oxidation resistance and thermal stability at high temperatures to minimize deposit formation and provide long service life. It has high load-carrying capacity to protect against wear. It protects system components against rust and corrosion, and is resistant is excessive foam buildup that can interfere with proper lubrication. It has a high viscosity index and a very low pour point for use over a wide temperature range.

Applications:

  • Land-based gas turbines
Syncon Turbine Oil meets the requirements of the following OEM specification:
  • Solar Turbines ES 9-224, Revision W, Class I (Synthesized Hydrocarbon) Turbine Oil
Features/Benefits:
  • Outstanding oxidation resistance and thermal stability at high temperatures
  • Excellent low-temperature fluidity
  • High viscosity index and very low pour point for use over a wide temperature range
  • Low volatility for lower oil consumption and less makeup oil
  • Protects against wear
  • Protects against rust and corrosion
  • Good foam resistance
  • Extended service intervals compared with conventional mineral oil-based lubricants

Information provided by Phillips 66 Lubricants.

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Viscosity Measurement, Index
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Oxidative Stability, ASTM D2272, RPVOT
  • ASTM Color, ASTM D1500
  • Total Acid Number, ASTM D974, [mg KOH/g]
  • Four Ball Wear, ASTM D4172, Scar Diameter
  • Pour Point
  • Flash Point, COC
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.