The styrene (alpha-methyl styrene)-butadiene SBR 1500 rubber is produced by emulsion copolymerization of styrene and butadiene at 4 – 8 C. The mixture of soaps of disproportionated rosin and synthetic fatty acids is used as emulsifier. It is well mixing with different ingredients of rubber compounds and is easily treated on the simple rubber production equipment, is well compatible with different rubbers of general use and needs no special plastification. It has higher strength properties and better metal adhesion. In mixing with SBR – 1712 at 1:1 rate the product will be of higher hardness, will grow tires abrasion resistance and will make bigger its running time up to 10%. Application: The SBR1500 is general purpose rubber. It is widely used in tyre, rubber technical, shoe, cable and other industries for production of automobile tires and tubes, wide assortment of rubber technical articles, white and color shoes, cable castings and so on. Information provided by Ganpati Exim PVT. LTD. |