MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Evonik VESTAMID® 1900GF20 BK 2.7206 PPE, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, 20% Glass Filled

Material Notes: VESTORAN® 1900GF20 BK 2.7206 is the registered trademark of Evonik Degussa GmbH for molding compounds containing poly-2,6-dimethyl-1,4-phenylene ether as polymeric constituent (polyphenylene ether, PPE, also referred to as PPO). As a material of amorphous structure VESTORAN® 1900GF20 shows very small mold shrinkage. Therefore molded parts have a very low tendency to warp. Moldings of VESTORAN® 1900GF20 are dimensionally stable and hydrolysis resistant even in hot water, but are more sensitive to organic solvents than semi-crystalline plastics. VESTORAN® 1900GF20 is resistant to aqueous alkalines and acides, certain alcohols, and glycol solutions. Glass fiber reinforcement of this molding material combines outstanding heat deflection temperature under load with high strength and rigidity. The even smaller shrinkage compared to non-reinforced VESTORAN® depends on the orientation of the glass fibers in the molded parts. VESTORAN® 1900GF20 is particularly suitable for the adhesion promoter-free manufacturing of plastic/rubber composites by the Evonik Degussa GmbH-patented K&K process ("direct-bonding to rubber"). Compared to VESTORAN® 1900, VESTORAN® 1900GF20 offers higher rigidity and strength. Colored material contains only cadmium-free pigments.
Dry properties listed below
Industrial Sector: Automotive and Mobility
Processing: Injection molding, Extrusion
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), Hydrolysis / hot water
Conformity: Automotive
Additives: Glass fibers
Processing: Profile extrusion, Sheet extrusion, K&K process
Special Characteristics: Amorphous, High heat resistant, Low warpage / Low shrinkage
Color: Black
Chemical Resistance: Acid resistance, Alkali resistance

Information provided by Evonik.

Vendors:
Available Properties
  • Density, ISO 1183
  • Water Absorption, Sim to ISO 62
  • Linear Mold Shrinkage, Flow, ISO 294-4, 2577
  • Linear Mold Shrinkage, Transverse, ISO 294-4, 2577
  • Melt Flow, ISO 1133
  • Tensile Strength at Break, ISO 527
  • Tensile Strength, ISO 527
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527
  • Elongation at Yield, ISO 527
  • Tensile Modulus, ISO 527
  • Flexural Modulus, ISO 178
  • Charpy Impact Unnotched, ISO 179/1eU, Type of failure: C
  • Charpy Impact, Notched, ISO 179/1eA, Type of failure: C
  • Charpy Impact, Notched, ISO 179/1eA, Type of failure: C
  • Tensile Impact Strength, ISO 8256/1, NOTCHED
  • Tensile Creep Modulus, 1 hour, ISO 899-1
  • Tensile Creep Modulus, 1000 hours, ISO 899-1
  • Volume Resistivity, IEC 62631-3-1
  • Surface Resistance, IEC 62631-3-2, RSD
  • Surface Resistance, IEC 62631-3-2, sE
  • Dielectric Constant, IEC 62631-2-1
  • Dielectric Constant, IEC 62631-2-1
  • Dielectric Strength, Sim. To IEC 60243-1, AC, S20/P50
  • Dissipation Factor, IEC 62631-2-1
  • Dissipation Factor, IEC 62631-2-1
  • Comparative Tracking Index, IEC 60112, test solution A, 50 drops value
  • CTE, linear, Parallel to Flow, ISO 11359-1/-2
  • CTE, linear, Transverse to Flow, ISO 11359-1/-2
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1/-2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
  • Vicat Softening Point, ISO 306, 50 K/h
  • Vicat Softening Point, ISO 306, 50 K/h
  • Glass Transition Temp, Tg, ISO 11357-1/-2
  • Flammability, UL94
  • Flammability, UL94
  • Oxygen Index, ISO 4589-1/-2
  • Oxygen Index, ASTM D2863
  • Melt Temperature, ISO 294, Injection Molding
  • Melt Temperature
  • Mold Temperature, ISO 294, Injection Molding
  • Mold Temperature
  • Injection Velocity, ISO 294, Injection Molding
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.