MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
3M Dyneon™ TF 2073Z PTFE Fine Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); PTFE Powder

Material Notes: Dyneon™ TF 2073 Z PTFE is an ideal grade for the manufacture of high quality micro tubing as well as wire and cable insulations. This product is also ideal for very thin-wall, smallest diameter tubing with maximum reduction ratio of up to 4200:1.

Product Features:

  • Needs less lubricant than TF 2072 Z PTFE
  • Emulsion polymerization PTFE
  • Product grade with lower extrusion pressure than TF 2070 Z PTFE
  • Wide processing range
  • Processing by standard paste extrusion methods
  • Meets ASTM D4895-04 Type 1, Grade 1, Class C classification
  • High molecular weight

Information provided by 3M

Vendors:
Available Properties
  • Bulk Density, DIN EN ISO 60
  • Density, DIN EN ISO 12086
  • Particle Size, ISO 13320
  • Tensile Strength at Break, DIN EN ISO 527-3
  • Elongation at Break, DIN EN ISO 527-3
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.