MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Eastman Provista UVO Copolymer
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Provista UVO is a Provista copolymer with an indoor/outdoor UV package added to prevent yellowing caused by light. Provista copolymer is a resin specifically developed for extrusion into profiles where aesthetics like high clarity and gloss, coupled with design flexibility drive demand. Compared to commonly used materials, Provista copolymer can often run on most standard processing equipment at increased speeds. An extremely high melt strength makes the resin an excellent choice when extruding profiles into complicated shapes. This product is certified to ANSI/NSF Standard 51.

Applications/Uses

  • Candy Packaging
  • Pricing channels
  • Tubing
  • Point of purchase displays
  • Food packaging
  • Furniture/furniture trim
  • Teething rails
  • Key Attributes

  • Ease of processing
  • Excellent chemical resistance
  • Sparkling clarity and high gloss
  • Toughness with flexibility
  • Vendors:
    Available Properties
    • Specific Gravity, ASTM D792
    • Hardness, Rockwell R, ASTM D785
    • Tensile Strength at Break, ASTM D638
    • Tensile Strength, Yield, ASTM D638
    • Elongation at Break, ASTM D638
    • Elongation at Yield, ASTM D638
    • Flexural Strength, ASTM D790
    • Flexural Modulus, ASTM D790
    • Izod Impact, Notched, ASTM D256
    • Izod Impact, Notched, ASTM D256
    • Izod Impact, Unnotched, ASTM D4812
    • Izod Impact, Unnotched, ASTM D4812
    • Puncture Energy, ASTM D3763, Puncture Resistance @Max Load, 23°C
    • Puncture Energy, ASTM D3763, Puncture Resistance @Max Load, 0°C
    • Puncture Energy, ASTM D3763, Puncture Resistance at Max Load
    • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
    • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
    • Vicat Softening Point, ASTM D1525, 1kg load
    • Haze, ASTM D1003
    • Gloss, ASTM D2457, at 60°
    • Transmission, Visible, ASTM D1003, Regular Transmittance
    • Transmission, Visible, ASTM D1003, Total Transmittance
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    Eastman Chemical Company

    Category Notes
    Plastic

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Visit Zeus Inc. for PEEK Tubing
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.