MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
3D Systems LaserForm® CoCr (B), AS-BUILT Cobalt-Chrome Alloy
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Cobalt Alloy

Material Notes: Cobalt-chromium-molybdenum alloy fine-tuned for use with DMP Flex 100, ProX® DMP 200 and ProX® DMP 300 metal printers producing industrial parts with high corrosion and wear resistance that also require high temperature resistance. LaserForm CoCr (B) is formulated and fine-tuned specifically for 3D Systems DMP Flex 100, ProX® DMP 200 and ProX® DMP 300 metal 3D printers to deliver high part quality and consistent part properties.

Cobalt-chromium-molybdenum alloys are known for their high strength and hardness and retain these properties even at elevated temperatures. In addition, they spontaneously form a protective passive film, which makes LaserForm CoCr (B) both corrosion resistant and biocompatible. These benefits make LaserForm CoCr (B) the ideal material for medical tools and devices, molds and dies, industrial, high wear applications and parts requiring high strength at elevated temperatures.

Classification: The chemical composition of LaserForm® CoCr (B) conforms to the requirements of the ASTM F75.

Information provided by 3D Systems

Vendors:
Available Properties
  • Density, Absolute theoretical
  • Hardness, Rockwell C, ASTM E18
  • Tensile Strength, Ultimate, ASTM E8M, Vertical direction - Z
  • Tensile Strength, Ultimate, ASTM E8M, Horizontal direction - XY
  • Tensile Strength, Yield, ASTM E8M, Rp0.2%, Vertical direction - Z
  • Tensile Strength, Yield, ASTM E8M, Rp0.2%, Horizontal direction - XY
  • Elongation at Break, ASTM E8M, Horizontal direction - XY
  • Elongation at Break, ASTM E8M, Vertical direction - Z
  • Reduction of Area, ASTM E8M, Horizontal direction - XY
  • Reduction of Area, ASTM E8M, Vertical direction - Z
  • Tensile Modulus, Youngs, Vertical direction - Z
  • Tensile Modulus, Youngs, Horizontal direction — XY
  • Electrical Resistivity
  • CTE, linear
  • Thermal Conductivity
  • Melting Point
  • Beryllium, Be
  • Cadmium, Cd
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co, Balance
  • Iron, Fe
  • Lead, Pb
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Silicon, Si
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
3D Systems Corporation

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.