| Hostacom PPU X9067HS PX7 NUTRIABEIGE is a medium high flow, medium flexural modulus HCPP copolymer resin with high toughness that is typically used for automotive interior trim applications. Availability: North America Application: Automotive Parts; Interior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Copolymer; Good Stiffness; Good Toughness Information provided by LyondellBasell. |