MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Petroquimica Triunfo Trithene® TS 3003 LDPE - Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: The Trithene® TS 3003 resin is a low-density, high molecular weight polyethylene that offers high mechanical strength and excellent optical properties. The product shows high modulus of elasticity, that it offers the property of recovering the original shape when finished the deformation strength. Additionally, because of its molecular structure, Trithene® TS 3003 resin shows excellent performance in conventional extruders and low energy consumption during processing, allowing the production of films with high thickness uniformity and good appearance. The additive package warrants thermal stability, low blocking, and adequate coefficient of friction - COF, which are required to allow high productivity on the extrusion, printing and finishing lines. This product complies with ASTM standard D1248-IIA5 and the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff.

Applications: Film for sleeve label to different kinds of bottles (soft drink, milk, mineral water, eatable oil, lubricants and hygiene products and cleanness). Shrink film with high gloss and mechanical strength. Grade for very stiff and transparent film.

Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.

Information provided by Dax Resinas

Key Words: FDA: 21 CFR 177.1520 (C) 2.1
Vendors:
Available Properties
  • Density, ASTM D1505
  • Thickness
  • Melt Index of Compound, ASTM D1238
  • Tensile Strength at Break, ASTM D638
  • Tensile Strength, Yield, ASTM D638
  • Film Elongation at Break, MD, ASTM D882
  • Film Elongation at Break, TD, ASTM D882
  • Elongation at Break, ASTM D638
  • Secant Modulus, MD, ASTM D882, 5%
  • Secant Modulus, TD, ASTM D882, 5%
  • Coefficient of Friction, Dynamic, ASTM D1894
  • Elmendorf Tear Strength, MD, ASTM D1922
  • Elmendorf Tear Strength, TD, ASTM D1922
  • Dart Drop Test, ASTM D1709, (method A)
  • Film Tensile Strength at Break, MD, ASTM D882
  • Film Tensile Strength at Break, TD, ASTM D882
  • Melting Point, ASTM D3418
  • Gloss, ASTM D2457, @ 60° Gardner
  • Transmission, Visible, transparent; thickness not quantified
  • Processing Temperature, Plasticizing Zone
  • Processing Temperature, Mixture Zone
  • Feed Temperature
  • Adapter Temperature
  • Die Opening
  • Blow-up Ratio (BUR), Recommended
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.