MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Flame Retardant adhesives
Caplinq LINQTAPE™ PIT1N-Alum 1-mil Polyimide Film with Sputtered Aluminized Coating
Categories: Polymer; Adhesive; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: CAPLINQ Linqstat™ PIT1N-Alum Series is a high performance, high-temperature resistant aluminized polyimide film, formed by sputtering aluminum on to polyimide using an aluminum vacuumed position method. This combination of materials allows that one side is an insulation side and the other is conductive. CAPLINQ Linqstat™ PIT1N-Alum Series combines these two materials to give a very heat resistant, mechanically and chemically stable, radiation-resistant, and self-extinguishing product that has very high thermal conductivity and EMI shielding. CAPLINQ Linqstat™ PIT1N-Alum Series is a used in a number of applications, including as a first surface mirror for multi layer insulation (MLI) blankets, EMI shielding, electromagnetic shielding tape and flexible etching wire.

Applications:

  • Best absorption/ emittance/ cost combination
  • Cost effective radiative transfer barrier
  • Excellent high temperature stability
  • Excellent burn resistance
  • Multilayer Insulation (MLI) blankets
  • EMI shielding
  • Flexible Etching Wire
  • First or second surface mirror

Information provided by Caplinq

Vendors:
Available Properties
  • Thickness, Aluminum Coating
  • Thickness, Film (Backing)
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Surface Resistivity per Square, Aluminum
  • Surface Resistivity per Square
  • Maximum Service Temperature, Inert, Intermittent
  • Maximum Service Temperature, Inert, Continuous
  • Minimum Service Temperature, Air, Intermittent
  • Minimum Service Temperature, Air, Continuous
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Flame Retardant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.