MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
CoreLite Board® Closed-Cell PVC Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoplastic; Vinyl (PVC); PVC, Foam Grade

Material Notes: CoreLite Board® is a cost-effective closed-cell PVC foam specially formulated to provide high physical properties and be recyclable. Engineered to meet the physical demands needed in transoms, attachment points, floors, bulkheads, stringers, local reinforcements, molds and tooling. CoreLite Board® is a stand-alone product and can be used without skins as a replacements for wood and plywood. This PVC foam has excellent fastener pullout strength and high flexural strength and stiffness. CoreLite Board® is 27% lighter than plywood.

Standard length and width 96" x 48". Property data reported parallel to the plane.

Information provided by CoreLite.

Vendors:
Available Properties
  • Density, ASTM C271, 10% Tolerance
  • Water Absorption
  • Tensile Strength, ASTM C297
  • Elongation at Break
  • Flexural Strength, ASTM D790
  • Compressive Strength, ASTM D1621
  • Compressive Modulus, ASTM D1621-B
  • Shear Modulus, ASTM C273
  • Shear Strength, ASTM C273
  • Peel Strength, ASTM D1062
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.