| Petrothene LR734002 is a high density polyethylene resin that exhibits good stiffness and environmental stress crack resistance. Typical applications include bottles for household chemicals, food products, and personal care products. Availability: North America Application: Bottles For Consumer Goods Market: Rigid Packaging Processing Method: Extrusion Blow Molding Attribute: Excellent Processability Information provided by LyondellBasell. |