MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Evonik VESTAMID® LX9013 BK 9.7507 Nylon 12, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® LX9013 BK 9.7507 is a plasticized polyamide 12 compound with an especially high long-term resistance under thermal load. The material absorbs only little moisture, thus leading to nearly unaffected dimensions and properties of the finished parts at changing ambient conditions. Extruded tubes are impact-resistant also at low temperatures. VESTAMID® LX9013 BK 9.7507 is suited to produce flexible tubes that are permanently exposed to higher temperatures, e.g., in the engine compartment of motor vehicles. Especially when used as diesel fuel lines they show significant advantages compared with standard grades, obvious in storage tests with diesel fuel (see the figure). The material corresponds to the extrusion compound PA12-HIPHL, grade1 acc. DIN 73378 and meets the requirements acc. DIN 74324 (black), ISO 7628 and SAE J844. VESTAMID® LX9013 BK 9.7507 is supplied as pellets in moisture-proof packaging ready for processing. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C
Industrial Sector: Automotive and Mobility, Sustainable
Sustainability: Sustainable electricity
Processing: Extrusion
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), UV / light / weathering, Oil / fuels
Electrical: Insulating
Conformity: Automotive
Additives: Unfilled
Applications: Tube and hose
Processing: Profile extrusion, Pipe/Tube extrusion
Special Characteristics: High impact strength, High heat resistant, High viscosity
Color: Black
Additives: Plasticizer, Impact restistant, Heat stabilizer
Delivery form: Fuel resistance

Information provided by Evonik.

Vendors:
Available Properties
  • Density, ISO 1183
  • Water Absorption, Sim to ISO 62
  • Moisture Absorption, Sim to ISO 62
  • Linear Mold Shrinkage, Flow, ISO 294-4, 2577
  • Linear Mold Shrinkage, Transverse, ISO 294-4, 2577
  • Hardness, Shore D, ISO 7619-1
  • Tensile Strength at Break, ISO 527
  • Tensile Strength, ISO 527
  • Tensile Stress, ISO 527
  • Elongation at Break, ISO 527, Nominal
  • Tensile Modulus, ISO 527
  • Flexural Strength, ISO 178, at conv. Deflection
  • Flexural Modulus, ISO 178
  • Flexural Strain at Break, ISO 178, at flexural strength
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact, Notched, ISO 179/1eA, Type of failure: C
  • Charpy Impact, Notched, ISO 179/1eA, Type of failure: P
  • Impact, SAE J2260, J2043, Cold impact resistance, breaks of 10, 912g;
  • Impact, SAE J844, Cold impact resistance, breaks of 10, 454g;
  • Impact, SAE J844, Cold impact resistance, breaks of 10, 454g; Pretreatment: 2h boiling water;
  • Impact, SAE J844, Cold impact resistance, breaks of 10, 454g; Pretreatment: 24h 110°C;
  • Impact, DIN 73378, with pendulum, pipe; Tube dimension: OD x WT 8x1 mm
  • Volume Resistivity, IEC 62631-3-1
  • Dielectric Constant, IEC 62631-2-1
  • Dielectric Constant, IEC 62631-2-1
  • Dielectric Strength, Sim. To IEC 60243-1, AC, S20/P50
  • Dielectric Strength, IEC 60243-1, AC, S20/S20, t.
  • Dissipation Factor, IEC 62631-2-1
  • Dissipation Factor, IEC 62631-2-1
  • Comparative Tracking Index, IEC 60112, test solution A, 50 drops value
  • CTE, linear, Parallel to Flow, ISO 11359-1/-2
  • CTE, linear, Transverse to Flow, ISO 11359-1/-2
  • Melting Point, ISO 11357-1/-3
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1/-2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
  • Vicat Softening Point, ISO 306, 50 K/h
  • Vicat Softening Point, ISO 306, 50 K/h
  • Glass Transition Temp, Tg, ISO 11357-1/-2
  • Flammability, UL94, IEC 60695-11-10
  • Flammability, UL94, IEC 60695-11-10
  • Melt Temperature, ISO 294, Injection Molding
  • Mold Temperature, ISO 294, Injection Molding
  • Injection Velocity, ISO 294, Injection Molding
  • Injection Pressure, ISO 294, Injection Molding
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.