MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Westlake EMAC® SP 1205 Ethylene-Methyl Acrylate Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Coating Grade

Material Notes: 20% Methyl Acrylate Content. Characteristics: Processing Temperature Range: 280-600°F, Less Crystalline and Softer than Polyethylene, Excellent Thermal Stability Allows Extrusion Processing up to 600°F, Non-Corrosive at Extrusion Temperatures, FDA Clearance for Packaging of Most Foods - including Aseptic Packaging, No FDA thickness limitation

Applications:Coatings & Laminations: Higher Neck-In but Similar Drawdown vs. LDPE Extrusion Coating Grades, Excellent Heat Seal Response at Low Seal Temperatures, Adheres Very Well to Non-Porous Substrates such as OPP, PVDC Coated Substrates, and Polyester, Adheres well to Porous Substrates such as Paper and Paperboard; Compounding: Impact Modification, Compatibilizer; Film: Tie Layers for LDPE, LLDPE, HDPE, PET, PP, PVDC, Ionomer, EVA, EAA, PVC (Rigid), PC

Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.

Vendors:
Available Properties
  • Density, ASTM D1505
  • ESCR 10% Igepal®, ASTM D1693, F50
  • Melt Flow, ASTM D1238, Cond. E
  • Hardness, Shore A, ASTM D2240
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength, Ultimate, ASTM D638
  • Elongation at Break, ASTM D638
  • Melting Point, by DSC
  • Vicat Softening Point, ASTM D1525
  • Brittleness Temperature, ASTM D746
  • Processing Temperature, Blown Film
  • Processing Temperature, Molding
  • Processing Temperature, Extrusion Coating
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Westlake Chemical Corporation

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.