Made by suspension polymerization.
APPLICATIONS
Extrusion : plasticized PVC
- profiles, tubes
- cables
- films and sheets
Calendering : plasticized PVC
- film
Injection molding : plasticized PVC Information provided by SolVin. SolVin is a predecessor company to Inovyn. |