VESTAKEEP® i4 3DF is a filament extruded from natural colored, high viscosity VESTAKEEP® i4 G polyether ether ketone (PEEK) resin. The material is especially designed for long term implantable medical devices. Dry properties listed below Industrial Sector: Medical Devices, 3D Printing Processing: 3D Printing Delivery form: (Mono)filament Resistance to: Heat (thermal stability), Hydrolysis / hot water, Wear / abrasion Conformity: Biocompatibility, Medical application Additives: Unfilled Applications: Monofilament Processing: Fused deposition molding Special Characteristics: Semi-crystalline Regulatory: US Pharmacopeia Class VI conformity Color: Natural color Chemical Resistance: Acid resistance, Alkali resistance, Solvent resistance, Grease resistance, Hydrolytically stable, Oil resistance, General chemical resistanceInformation provided by Evonik. |