MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Master Bond EP21TDCHTND Versatile, toughened two component epoxy for bonding, sealing and coating
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Product Description: Master Bond EP21TDCHTND is a two component epoxy adhesive, sealant and coating featuring high performance, versatility and exceptional user friendliness. It has a very forgiving and convenient one to one mix ratio by weight or volume. It cures at ambient temperatures that can be accelerated by adding heat, with the optimum cure schedule being overnight at room temperature, followed by 1-2 hours at 150-200°F. This non-drip viscosity system bonds well and with minimum shrinkage to a wide variety of substrates including metals, composites, glass, ceramics and many plastics and rubbers. EP21TDCHTND combines good dimensional stability with toughness. The forgiving nature of EP21TDCHT allows it to be used for bonding dissimilar substrates that might have different coefficients of thermal expansion, conferring upon it top notch resistance to rigorous thermal cycling as well as vibration and shock. Additionally, it is a superior electrical insulator and has good chemical resistance against water, fuels and oils. Its wide service temperature range is from -100°F to +350°F. Both Parts A and B are amber in color. It can be used in aerospace, electrical, electronic, medical, specialty OEM and a wide variety of other industries as well.

Product Advantages:

  • Convenient mixing: non-critical equal weight or volume ratio
  • User friendly, easy to apply, smooth paste along with convenient curing schedules
  • Impressive adhesion to a wide variety of substrates
  • Superior toughness, can withstand harsh thermal cycling while retaining dimensional stability
  • Dependable electrical insulation values
  • Robust temperature resistance profile from -100°F to +350°F

Information provided by MasterBond®

Vendors:
Available Properties
  • Hardness, Shore D
  • Tensile Strength at Break
  • Tensile Modulus
  • Shear Strength, Al/Al, Tensile lap
  • Peel Strength, T-peel
  • Volume Resistivity
  • Dielectric Constant
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time, Followed by 2-3 hours at 150-200°F (Optimum Cure Schedule)
  • Cure Time
  • Pot Life, 100 gram mass
  • Shelf Life, in original unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.