MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Ravago Manufacturing Americas Aquatuf® HMP-337 (Roto) HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: HMP-337 is a high-density polyethylene compound designed for applications like kayaks or boats that require a balance high stiffness and extreme toughness.

Key Features: 35-mesh powder; Good moldability; Excellent long term outdoor weatherability (UV15); Superior balance of toughness and rigidity; Very high stiffness; Excellent low temperature impact; Compounded for uniform additive dispersion; Natural as well as standard, custom or special effect colors available; Stock colors may be available. See Stock color bulletin; Also available in pellet form as HM-337

Availability: North America

Features: Good Moldability; Good Toughness; Good Weather Resistance; High Rigidity; High Stiffness; Low Temperature Impact Resistance

Appearance: Colors Available; Opaque

Form: Powder

Processing Method: Rotational Molding

Information provided by Ravago Manufacturing Americas

Vendors:
Available Properties
  • Bulk Density, ASTM D1895, 35-mesh powder
  • Density, ASTM D792
  • Melt Flow, ASTM D1238
  • Flexural Modulus, ASTM D790, Tangent, Rotational Molded
  • Impact Test, Rotational Molded, F50
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Unannealed, Rotational Molded
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Unannealed, Rotational Molded
  • Flammability, UL94
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.