| Description: This is a non-corrosive, neutral cure, 1-part, RTV (Room Temperature Vulcanizing) silicone adhesive sealant. It is one in a range of Alkoxy cure products which are solvent free. It exhibits excellent primerless adhesion to many substrates and cures at room temperature when in contact with atmospheric moisture to form a tough rubber. This product will not corrode copper or its alloys and is suitable for use with electronic components. Key Features - Thermally conductive
- Non corrosive for sensitive substrates
- Low thermal outgassing (ECSS-Q-ST-70-02C)
- UL94 V0 recognized in file No. E334038
Application: Electronic assemblies, aerospace and automotiveInformation provided by CHT Group |