MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Master Bond MasterSil 156 Two Part, Low Viscosity Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: Master Bond MasterSil 156 is a two component, lower viscosity silicone system for high performance potting, encapsulation and sealing. MasterSil 156 combines high temperature resistance, commendable flexibility and appealing thermal conductivity along with meeting UL 94V-0 for flame retardancy. MasterSil 156 is an addition cured system and does not require exposure to air for complete cross-linking. It has a convenient one to one mix ratio by weight and will not outgas while curing. It is 100% solids and contains no solvents. MasterSil 156 has a lower viscosity and excellent flow properties enabling it to be well suited for potting and encapsulation. Additionally, the electrical insulation properties are good and it still is a reputable thermal conductor. It bonds well to a wide variety of substrates including metals, composites, glass, ceramics and many rubbers and plastics. Its flexibility allows it to withstand severe thermal cycling and resist vibration and shock. Also, it is very resistant to water, humidity, oils and environmental elements. The system is rated to 105°C by UL in thicknesses up to 1/4 inch and above, and it is listed as 94V-0 for flame retardancy. It can cure in thicknesses well beyond 1-2 inches if required. MasterSil 156 is a system that combines flexibility, high temperature resistance, heat dissipation and flame retardancy.

Product Advantages:

  • Convenient one to one by weight mix ratio
  • Addition cured; virtually no by-products released during curing; does not require air
  • Favorable electrical insulation and thermal conduction properties
  • Lower viscosity and splendid flow; ideal for potting and encapsulation
  • Very low shrinkage upon cure
  • UL flame retardant 94V-0 rating
Key Features
  • Good thermal conductivity
  • Good electrical insulation properties
  • Flame retardant UL 94V-0
  • Low exotherm; very long pot life
  • Can cure in thicknesses up to and beyond 1-2 inches
  • UL temperature rated up to 105°C

Information provided by MasterBond®

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, Part A
  • Hardness, Shore A
  • Tensile Strength at Break
  • Elongation at Break
  • Shear Strength, Tensile lap, Al to Al
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Flammability, UL94
  • Cure Time
  • Cure Time
  • Pot Life, 100 gram batch
  • Shelf Life, in original unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.