| Hostacom EKC 330N E1 C12A19 is a 16% talc filled PP copolymer, with excellent impact/stiffness balance, good flowability, good scratch resistance and outstanding blooming resistance at elevated temperatures. Product is available as a customized color matched, pellet form. This grade is delivered in C12A19 color version. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Europe Application: Automotive Parts; Interior Trims Market: Automotive Processing Method: Injection Molding Attribute: Excellent Processability; Good Processability; High Impact Resistance; Scratch Resistant; UV Resistant Information provided by LyondellBasell. |