| Metal coated SSAB Domex structural steels are widely used by construction industry in various building components, for example in load-bearing sheets and corrugated profiles, purlins and nail plates. The product offering features metal coated structural steels in grades with a minimum yield strength from 220 to 350 MPa with Zinc (Z), Galfan (ZA) or Galvannealed (ZF) coating. Galvanic corrosion protection of metal coated SSAB Domex enables a long service life for end products that are used under corrosive conditions. This makes these metal coated grades ideal for big installations, like solar panel racks or silos. These steel grades comply with EN 10346 standard and exceed the standard requirements by better formability and more consistent properties, which increase the productivity in workshop thanks to the stable forming result. SSAB Domex 250GD meets and exceeds the requirements of S250GD in EN 10346. Dimension Range: SSAB Domex 250GD is available in thicknesses of 0.45-3.00 mm and widths up to 1520 mm as coils, slit coils and as cut to length in lengths up to 6 meters. Available dimensions depend on the coating. Data provided by SSAB. |