| Popular alloy with score resistance, structural uniformity, shear properties, compressive strength and low cost. Applications: Bearings, bushings, sleeves, liners, piston rings, hydraulic parts Information provided by MetalTek Cast UNS C94100; Cast Grade C94100; Cast ASTM B66; Mil QQ-C-390B |