MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Lanxess THERBANĀ® AT 3904 VP Butadiene Acrylonitrile Copolymer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: A low viscosity, fully hydrogenated butadiene acrylonitrile copolymer (less than 1% residual double bonds), which provides vulcanizate with superior resistance to heat, ozone and excellent resistance to non-polar hydrocarbon fluids including those containing aggressive additives. With this level of unsaturation, Therban AT 3904 VP-based compounds can only be vulcanized with peroxides or high-energy radiation. The incorporation of a crosslinking co-agent is recommended for optimized physical properties of both unaged and aged vulcanizates. Low viscosity AT-technology provides a broad processing window, low mold fouling and the potential for higher filler loads compared to standard viscosity HNBR types.

Information provided by Lanxess.

Vendors:
Available Properties
  • Density
  • Volatiles, ASTM D5668
  • Mooney Viscosity, ASTM D1646, (1+4)
  • Ash, ASTM D5667
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Lanxess, Spinoff of Bayer

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.