MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
LG Chemical LUTENE® XL2902BK Semi-conductive compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Applications: Excellent-smoothness extra clean semi-conductive compound for conductor and bonded insulation shielding of high voltage power cable

Description:

  • LUTENE® XL2902BK is a cross-linkable semi-conductive shielding compound for conductor and bonded insulation shielding of high and extra high voltage power cables.
  • LUTENE® XL2902BK is compatible with both copper and aluminum conductors. LUTENE® XL2902BK was specifically developed to provide a super-smooth surface yielding a more perfect interface between extruded shield and the insulation. As a result, significantly improved cable performance can be expected.
  • LUTENE® XL2902BK has stable volume resistivity characteristics at elevated temperature. Characteristics:
    Excellent Surface Smoothness
    Excellent Electrical Properties
    Excellent Physical and Thermal Properties
    Long-run Extrusion without Scorch
    Contaminant Free

    Specification: LUTENE® XL2902BK meets the property requirement of the following material specifications.
    AEIC CS8
    AEIC CS 7-96
    IEC 60502, 60840, 62067
    ICEA S-94-649, S-66-524 / NEMA WC74

    Information provided by LG Chemical

  • Vendors:
    Available Properties
    • Density, ASTM D1505, Base Resin
    • Tensile Strength at Break, ASTM D638, 200?/min
    • Tensile Strength at Break, ASTM D638, retention after
    • Elongation at Break, ASTM D638, 200 mm/min
    • Elongation at Break, ASTM D638, retention after
    • Volume Resistivity, ASTM D991, DC
    • Volume Resistivity, ASTM D991, DC
    • Brittleness Temperature, ASTM D746, no crack
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    none

    Category Notes
    Plastic

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Visit Zeus Inc. for PEEK Tubing
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.