| Metal coated SSAB Domex HSLA steels are designed for demanding structural applications that require galvanic corrosion protection and good formability in addition to high strength. Metal coated SSAB Domex HSLA steels are designated according to their minimum guaranteed yield strength from 220 to 500 MPa. Most of these steel grades comply with EN 10346 standard and exceed the standard requirements by better formability and more consistent properties, which increase the productivity in workshops thanks to the stable forming result. A low variation in mechanical properties makes them highly suitable for automated forming processes. In addition to normal zinc (Z) coatings, the offering contains Galfan (ZA) and Galvannealed (ZF) coatings for enhanced level of corrosion protection. SSAB Domex 260LAD meets and exceeds the requirements of HX260LAD in EN 10346. Dimension Range: SSAB Domex 260LAD is available in thicknesses of 0.50-3.00 mm and widths up to 1520 mm as coils, slit coils and as cut to length in lengths up to 6 meters. Available dimensions depend on the coating. Data provided by SSAB. |