| Hifax TYC 852P T C12716 is a 22% talc filled impact modified polypropylene, with high flowability, high impact resistance and low CLTE. Product is available as a customized color matched, pellet form. This grade is delivered in C12716 color version. Status: Commercial – Active Availability: Asia-Pacific Application: Exterior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Good UV Resistance; High Flow; High Impact Resistance Information provided by LyondellBasell. |