MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
3D Systems LaserForm® Ti Gr23 (A), AFTER HIP Titanium
Categories: Metal; Nonferrous Metal; Titanium Alloy

Material Notes: Titanium alloy fine-tuned for use with ProX® DMP 320 metal powder producing technical and medical parts with a combination of high specific strength and excellent biocompatibility. LaserForm Ti Gr23 (A) is ELI (Extra Low Interstitial) grade with lower iron, carbon, and oxygen content and is known for higher purity than LaserForm Ti Gr5 (A) resulting in improved ductility and fracture toughness. LaserForm Ti Gr23 (A) is formulated and fine-tuned specifically for 3D Systems’ ProX DMP 320 metal 3D Printers to deliver highest part quality and best part properties. The print parameter database that 3D Systems provides together with the material has been extensively developed, tested and optimized in 3D Systems’ part production facilities that hold the unique expertise of printing 500,000 challenging production parts year over year. Based on over 1000 test samples the below listed part quality data and mechanical properties give you high planning security. And for a 24/7 production 3D Systems’ thorough Supplier Quality Management System guarantees consistent, monitored material quality for reliable process results.

Material Description: This titanium alloy is commonly used in aerospace and medical applications because of its high strength, low weight and excellent biocompatibility. The essential difference between Ti6Al4V ELI (grade 23) and Ti6Al4V (grade 5) is the reduction of oxygen content to 0.13% (maximum) in grade 23. This confers improved ductility and fracture toughness, with some reduction in strength. These benefits make LaserForm Ti Gr23 (A) the most used medical and aerospace titanium grade. It can be used in biomedical applications such as surgical implants, orthodontic appliances or in-joint replacements due to its biocompatibility, good fatigue strength and low modulus.

Classification: Parts built with LaserForm Ti Gr23 (A) Alloy have a chemical composition that complies with ASTM F3001, ISO 5832-3, ASTM F136 and ASTM B348 standards.

Information provided by 3D Systems

Vendors:
Available Properties
  • Density, Absolute theoretical
  • Hardness, Rockwell C, ASTM E18
  • Tensile Strength, Ultimate, ASTM E8M, Horizontal direction — XY
  • Tensile Strength, Ultimate, ASTM E8M, Vertical direction — Z
  • Tensile Strength, Yield, ASTM E8M, Rp0.2%, Horizontal direction - XY
  • Tensile Strength, Yield, ASTM E8M, Rp0.2%, Vertical direction - Z
  • Elongation at Break, ASTM E8M, Horizontal direction — XY
  • Elongation at Break, ASTM E8M, Vertical direction — Z
  • Reduction of Area, ASTM E8M, Horizontal direction — XY
  • Reduction of Area, ASTM E8M, Vertical direction — Z
  • Tensile Modulus, ASTM E8M, Young's
  • Fatigue Strength, ASTM E47
  • Charpy Impact, ASTM E23
  • CTE, linear
  • Thermal Conductivity
  • Melting Point
  • Aluminum, Al
  • Carbon, C
  • Hydrogen, H
  • Iron, Fe
  • Nitrogen, N
  • Oxygen, O
  • Titanium, Ti, Balance
  • Vanadium, V
  • Yttrium, Y
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
3D Systems Corporation

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.