| MORCHEM UD 5037F is an anionic, aliphatic structured polyester based polyurethane dispersion. This polyurethane dispersion distinguish itself by its elastic film hardness in the range of shore hardness 75-77A. This PU dispersion based on aliphatic distinguish itself by the excellent UV constancy and is the element raw material for producing divers aqueous polyurethane adhesives, adhesive coatings and adhesive equipment. This dispersion is also used as a lamination coating and as Top Coat in the textile coating. Furthermore this dispersion is also suitable for producing of leather finishes and leather covering color. Application: MORCHEM UD 5037F is applied to serve as a basic raw material by the production of aqueous 1- and 2-component adhesives. Adhesives and adhesive coatings which were produced with MORCHEM UD 5037F are especially good suitable for: - Textile lamination
- Coating of casings and profiles
- Lamination of thermoplastic foils with wooden materials as for instance by membrane press application
- Deep-draw and press lamination application for the automotive industry.
- Shoe soles- and shoe shank fitting
- Lamination of split leather and plastic foils. We recommend, for the processing of 2- component adhesives, the application of the cross link agent DANCURE 101.
Information provided by Danquinsa GMBH |