High hardness armor with extraordinary toughness properties. Armox 560T is the world’s toughest protection plate, having nominal 560 HBW hardness, for use in vehicles, buildings and many more applications. Benefits of Armox 560T include:- Market-leading steel protection
- Superior workshop properties
- Optimized solutions
- Perfect hardness/toughness balance, for combined penetration and blast protection
- Expertise in ballistic protection from SSAB