MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Northstar Polymers MPA-221 Polyether Based MDI Prepolymer
Categories: Polymer; Thermoset

Material Notes: MPA-221 is polyether based MDI prepolymer with 1.9% free NCO. The composition mole ratio between MDI to polyol is approximately 2:1, which theoretically makes prepolymer with molecular structure having a long polyol chain sandwiched by two NCO groups. The theoretical functionality of MPA-221 is very close to 2.0. This makes MPA-221 a good prepolymer to modify full-prepolymer systems and moisture cure systems to yield softer films. The polyether polyol used in this formulation is more apolar, and it has good affinity to a wide range of prepolymer species and good moisture permeation for moisture-cure adhesives and coatings. The viscosity of MPA-221 can be reduced to the range easier to process by heating.

Information provided by Northstar Polymers

Vendors:
Available Properties
  • Specific Gravity
  • Viscosity
  • Viscosity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.