MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
LyondellBasell Petrothene® NA940000 Low Density Polyethylene, Film Data
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Applications
PETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for bags used to package fertilizer, peat moss, decorative stone and agricultural and construction materials.

Regulatory Status
NA 940 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply.

Processing Techniques
NA 940 has been designed for excellent processability, bubble stability and good heat sealing over a wide range of extrusion conditions. Optimum properties are found at melt temperatures of 330°430°F and blow-up ratios between 1.8:1 and 2.5:1. Drawdown to 1.5 mil is possible at commercial rates when proper extrusion techniques are used. Specific recommendations for processing NA 940 can be made only when the end use applications, required properties and processing equipment are known.

Physical Properties
These are typical values and not to be construed as specific product limits. Data obtained from film produced in a 3.5"(89mm) blown film line, commercially available 8"(203 mm)die, 375°F(191°C) melt extrusion temperature, 2:1 BUR, 1.25 mil (32 micron) gauge, 0.025"die gap at 130 lb/hr.

This product is from the former Equistar product line.

Vendors:
Available Properties
  • Density, ASTM D1505
  • ESCR 100% Igepal®, ASTM D1693, Cond. A, 0 failures in 7 days
  • Thickness, 2:1 BUR; 25 mil die gap
  • Melt Flow, ASTM D1238
  • Antiblock Level
  • Slip Level
  • Hardness, Shore D, ASTM D2240, Molded
  • Tensile Strength, Yield, ASTM D638, Molded
  • Film Elongation at Break, MD, ASTM D882
  • Film Elongation at Break, TD, ASTM D882
  • Elongation at Break, ASTM D638, Molded
  • Flexural Modulus, ASTM D790, Molded
  • Elmendorf Tear Strength MD, ASTM D1922
  • Elmendorf Tear Strength TD, ASTM D1922
  • Dart Drop Test, ASTM D1709, F50
  • Film Tensile Strength at Break, MD, ASTM D882
  • Film Tensile Strength at Break, TD, ASTM D882
  • 1% Secant Modulus, MD, ASTM D882
  • 1% Secant Modulus, TD, ASTM D882
  • Vicat Softening Point, ASTM D1525
  • Brittleness Temperature, ASTM D746, Molded; F50
  • Melt Temperature
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
LyondellBasell LYB (former Equistar)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.