| ECO-FIL-A-GEHR Wood® consists of recycled wood fibers mixed with a recycled biopolymer. The raw material is made by Sulapac®. The printed material is haptic, visual and odor like wood. Nevertheless, it can be used to print extremely robust / stable parts Features: Highest precision in diameter and roundness; Filaments made of high-quality raw materials; Compatible with all open-system 3D printers; Low-emission and odor free; Void-free; Good layer adhesion; Ideal flow behavior while printing; Carefully spooled and packed in easy to use aluminum-laminated resealable zip bags Distinctive Features: Filaments made of high-quality and renewable raw materials; Haptic, visual and odor like wood; Food contact approval on the raw material; High dimensional stability; High modulus of elasticity; Pressure nozzle temperature 210°C, printing plate temperature 60°C Typical Applications: Cosmetic jar; Decorative components; Sustainable Displays Recycling: Box and spools are made of pure materials (PAP20 and PC) and are therefore recyclable through correct disposal. Information provided by GEHR Plastics, Inc. |