| The ballistic protection steel with extra-high hardness. Ramor 550 is a ballistic protection steel of extra-high hardness, available in thicknesses of 3.0 - 15.0 mm (0.118-0.591") and hardnesses of 540-600 HBW. Ramor 550 is available as cut-to-length sheet in thicknesses of 3.0 - 6.0 mm (0.118-0.236") and as plate in thicknesses of 6.0 - 15.0 mm (0.236-0.591"). Delivered in quenched condition, Ramor 550 is not intended for further heat treatment. Dimension Range: Ramor 550 is available as cut-to-length sheet in thickness between 3.0-6.0 mm, and as plate in thickness between 6.0 - 15.0 mm. Data provided by SSAB. |