| Base Polymer: Polyamide 66 Filler/Additive System: special filler Special Features: Electrically conductive, thermal conductive, heat ageing stabilization Market Segment: Automotive, Machinery, Electrical and Electronic, Lighting Application Area: Electrical components, radiator systems, cooling system Typical Application: Housings, functional components Information provided by Albis Plastics |