MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
SSAB Domex Tube Double Grade S355J2H Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel

Material Notes: SSAB Domex Tube Double Grade is structural hollow section. It meets or exceeds the requirements of standard EN 10219 and includes two separate modern steel grades: S355J2H and S420MH. The choice of grade depends on the customer's or designer's application and requirements. When your main goal is excellent usability or simplicity of design, grade S355 presents the best choice. If you are looking for considerable weight reduction and longer spans, consider selecting grade S420MH. Welding and other workshop instructions and regulations like welding procedure test (ISO 15614-1), material classification (ISO 15608), welding qualification (EN 287-1; ISO 9606-1) and EN 1090 certification procedure must follow the appropriate steel grade S355 or S420 selected. Welding in corner areas is always permitted when using SSAB steels.

Dimension Range: SSAB Domex Tube Double Grade is available in circular, square and rectangular shapes.

Data provided by SSAB.

Vendors:
Available Properties
  • Tensile Strength, Rm
  • Tensile Strength, Rm
  • Tensile Strength, Yield, Rp0.2
  • Tensile Strength, Yield, Rp0.2
  • Elongation at Break, A5
  • Elongation at Break, A5
  • Charpy Impact, 10x10 mm test specimen
  • Charpy Impact, 10x10 mm test specimen
  • Carbon, C
  • Iron, Fe, Balance
  • Manganese, Mn
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
SSAB Tunnplat AB

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.