MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
SEKISUI SPI KYDEX® T MB Thermoplastic sheet
Categories: Polymer; Thermoplastic

Material Notes: KYDEX® T MB is a proprietary thermoplastic sheet that is cost competitive with fire retardant ABS/PVC (FR-ABS) formulations but with significantly higher impact strength and extensibility. Antimicrobial protection is built-in to continuously fight the growth of microbes.

Since KYDEX® T MB is less hygroscopic, unlike FR-ABS, it typically does not require pre-drying, offers superior impact, more uniform forming with less wall thinning and offers significantly greater resistance to a broad range of corrosive chemicals and cleaning solutions. It is available in a wide range of aesthetic choices and is Underwriter’s Laboratories, Inc.® recognized Std 94 V-0, 5V.

Suggested Application:

  • Aircraft Interiors
  • Mass Transit Vehicle Interior Components
  • Equipment Housings
  • Medical Products
  • Kiosk Housings
Features:
  • Substitute for FR-ABS sheet with competitive pricing but superior cost/performance
  • Higher breakage resistance measured by the Notched Izod test than competitive thermoplastics
  • Available in thicknesses from 0.71mm (0.028”) and up, in eight textures, a variety of colors, custom blank sizes and low minimums
  • Among the most rigid of thermoforming materials with a modulus of elasticity of 2,482 MPa (360,000 psi)
  • Easy to form with excellent part definition and deep-draw characteristics
  • Recognized by Underwriter’s Laboratories, Inc® for Std 94 V-0, 5V in all thicknesses
  • Form times similar to FR-ABS making it an easy transition from competitive products.
  • Antimicrobial protection inhibits the growth of bacteria that can cause stains, odors and product deterioration.
  • Antimicrobial protection is built-in to the sheet so it won’t wash or wear away and lasts for the lifetime of the product/sheet.
  • Antimicrobial protection keeps the surface cleaner between cleanings.

Information provided by SEKISUI KYDEX, LLC.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Moisture Absorption, ASTM D570
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Yield Strength, ASTM D695
  • Compressive Modulus, ASTM D695
  • Bearing Yield Strength, ASTM D953
  • Bearing Yield Strength, ASTM D953
  • Poissons Ratio, ASTM D638
  • Shear Strength, ASTM D732
  • Izod Impact, Notched, ASTM D256
  • Gardner Impact, ASTM D5420, Drop Dart Impact, GE
  • Dielectric Strength, ASTM D149, oil
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, annealed
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.