MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Covestro Impranil® VP LS 2346 Polyacrylate Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Characterization: Polyacrylate resin; crosslinkable with melamine/formaldehyde. Impranil® VP LS 2346 is particularly suitable for the direct coating of polyamide fabrics and polyester blends used in the manufacture of rainwear and sportswear.

Properties / Applications: Drying and condensation (crosslinking) The first coats should be dried at a temperature of max. 100°C. Drying of basecoats at temperatures above 100 °C results in partial or even full crosslinking, which has an adverse effect on the adhesion between the basecoat and the topcoat. Coating delamination occurs as a result. The last coats can be dried at higher temperatures, e.g. 100 – 140 °C. The dried goods crosslink within one minute at 150 – 160 °C. If Impranil® VP LS 2346 is crosslinked with Imprafix® TH Lösung, there is no need for hot crosslinking after drying. The isocyanate reaction will then be completed after 2 to 3 days.

Information provided by Covestro

Vendors:
Available Properties
  • Volatiles, DIN EN ISO 3251, 0.9 - 1.1 g/1 h/125 °C/convection oven
  • Viscosity, DIN EN ISO 3219/A.3
  • Tensile Strength at Break, DIN 53504, after 14 d hydrolysis
  • Tensile Strength at Break, DIN 53504, after 400 h Xenotest
  • Tensile Strength at Break, DIN 53504, original
  • Elongation at Break, DIN 53504
  • 100% Modulus, DIN 53504
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Covestro Deutschland AG, Bayer MaterialScience

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.