MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Domo Technyl® A 60G1 V25 25% Glass Reinforced Nylon 66, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: This Red Phosphorous and Halogen free flame retardant grade, combines excellent all-round mechanical properties with outstanding flame retardancy (UL 5VA at 1.6mm) and electrical performance. This product is ideally suited for industrial controls and power distribution applications such as MCBs and contactors. The long term thermal performance of this grade also make it ideal for underhood auto applications where it can withstand temperatures of 160°C for over 6000hrs.

Information provided by Rhodia; Rhodia has been acquired by Solvay.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors:
Available Properties
  • Density, ISO 1183-A
  • Water Absorption, ISO 62
  • Linear Mold Shrinkage, Flow, ISO 294-4
  • Linear Mold Shrinkage, Transverse, ISO 294-4
  • Linear Mold Shrinkage, Transverse, Rhodia EP test
  • Tensile Strength at Break, ISO 527 Type 1 A, Conditioned
  • Tensile Strength at Break, ISO 527 Type 1 A, DAM
  • Elongation at Break, ISO 527 Type 1 A, DAM
  • Elongation at Break, ISO 527 Type 1 A, Conditioned
  • Tensile Modulus, ISO 527 Type 1 A, Conditioned
  • Tensile Modulus, ISO 527 Type 1 A, DAM
  • Charpy Impact Unnotched, ISO 179/1eU, DAM
  • Charpy Impact Unnotched, ISO 179/1eU, Conditioned
  • Charpy Impact Unnotched, ISO 179/fU, DAM
  • Charpy Impact, Notched, ISO 179/1eA, DAM
  • Charpy Impact, Notched, ISO 179/1eA, Conditioned
  • Volume Resistivity, IEC 60093, Conditioned
  • Volume Resistivity, IEC 60093, DAM
  • Surface Resistance, IEC 60093, Conditioned
  • Dielectric Constant, IEC 60250, DAM
  • Dielectric Constant, IEC 60250, Conditioned
  • Dielectric Strength, IEC 60243, DAM
  • Comparative Tracking Index, IEC 60112, Conditioned
  • Melting Point, ISO 11357
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75/Bf, DAM
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75/Af, DAM
  • Flammability, UL94, ISO 1210/UL94, DAM
  • Flammability, UL94, ISO 1210/UL94, DAM
  • Oxygen Index, ISO 4589, DAM
  • Glow Wire Ignition Temperature, IEC 60695-2-13, DAM
  • Glow Wire Ignition Temperature, IEC 60695-2-13, DAM
  • Glow Wire Flammability Index, IEC 60695-2-12, DAM
  • Glow Wire Flammability Index, IEC 60695-2-12, DAM
  • Glow Wire Flammability Index, IEC 60695-2-12, DAM
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Mold Temperature
  • Drying Temperature
  • Moisture Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.