MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Evonik VESTAMID® L2124 BK 9.7507 Nylon 12, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® L2124 BK 9.7507 is a plasticized, heat- and light- stabilized polyamide 12 compound for the extrusion of flexible tubing and hoses especially for oil and petrochemical applications. Tubing according to DIN 73 378, Type: PA 12-PHL. Properties of compounds based on PA 12 vary little with changing humidity due to low moisture absorption. Parts made of this semi-crystalline material are characterized by exceptional impact strength, low coefficient of friction and good chemical resistance. VESTAMID® L2124 BK 9.7507 is characterized by a high melt viscosity and good dimensional control during pipe extrusion. VESTAMID® L2124 BK 9.7507 is supplied as cylindrical granules, ready for processing, in moisture-proof bags. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Industrial Sector: Automotive and Mobility, Sustainable, Industry and Engineering
Sustainability: Sustainable electricity
Processing: Injection molding, Extrusion
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), UV / light / weathering, Oil / fuels
Electrical: Insulating
Conformity: Automotive
Additives: Lubricant, Unfilled
Processing: Profile extrusion, Pipe/Tube extrusion
Special Characteristics: Semi-crystalline, Light-stabilized, U.V. stabilized, High heat resistant
Features: Low coefficient of friction
Color: Black
Additives: Plasticizer, Light stabilizer, Heat stabilizer, Processing aids
Chemical Resistance: Oil resistance, General chemical resistance

Information provided by Evonik.

Vendors:
Available Properties
  • Density, ISO 1183
  • Tensile Stress
  • Tensile Stress
  • Tensile Stress
  • Tensile Stress
  • Tensile Stress
  • Tensile Stress
  • Tensile Stress
  • Tensile Stress
  • Tensile Stress
  • Tensile Stress
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527, Nominal
  • Elongation at Yield, ISO 527
  • Tensile Modulus, ISO 527
  • Tensile Modulus
  • Tensile Modulus
  • Flexural Strength, ISO 178, at conv. Deflection
  • Flexural Strength, ISO 178
  • Flexural Modulus, ISO 178
  • Flexural Strain at Break, ISO 178, at flexural strength
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact, Notched, ISO 179/1eA, Type of failure: C
  • Charpy Impact, Notched, ISO 179/1eA, Type of failure: C
  • Tensile Creep Modulus, 1 hour
  • Tensile Creep Modulus, 1 hour
  • Tensile Creep Modulus, 1 hour
  • Tensile Creep Modulus, 1 hour
  • Tensile Creep Modulus, 1 hour
  • Tensile Creep Modulus, 1 hour
  • Tensile Creep Modulus, 1 hour, ISO 899-1
  • Tensile Creep Modulus, 1000 hours
  • Tensile Creep Modulus, 1000 hours
  • Tensile Creep Modulus, 1000 hours
  • Tensile Creep Modulus, 1000 hours
  • Tensile Creep Modulus, 1000 hours
  • Tensile Creep Modulus, 1000 hours
  • Tensile Creep Modulus, 1000 hours, ISO 899-1
  • Volume Resistivity, IEC 62631-3-1
  • Surface Resistance, IEC 62631-3-2
  • Dielectric Constant, IEC 62631-2-1
  • Dielectric Constant, IEC 62631-2-1
  • Dielectric Strength, IEC 60243-1, AC, S20/S20, t.
  • Dissipation Factor, IEC 62631-2-1
  • Dissipation Factor, IEC 62631-2-1
  • Comparative Tracking Index, IEC 60112, test solution A, 50 drops value
  • Melt Temperature, ISO 294, Injection Molding
  • Mold Temperature, ISO 294, Injection Molding
  • Injection Velocity, ISO 294, Injection Molding
  • Injection Pressure, ISO 294, Injection Molding
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.