MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
EBS ACRALOCK FA10-05 Structural Methacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: Property data using FA10-05A A-component.

Flexible, low modulus adhesive up to 250% elongation after 82°C post cure bake cycle, low exothermic heat and less read-through, thick gap filling primerless on most metal s including aluminum and stainless steel.

Description: Flexible adhesive, primerless, low exotherm

Application:

  • Transportation-Bus/Truck/Rail
    • Grill/bumper
    • Aerofoil/cab assembly
    • Kick plates panel side strips
    • Dashboards
    • Wall corner joints
    • Roof to wall panels
    • Glove boxes/console
    • Door panel/door shins
    • Spoilers
    • Rail skins/pin potting
    • AL-FRP
    • Metal hinges/brackets
    • Bus-fram/skins/brackets
  • Marine-Applications:
    • Stringers
    • Deck to hull
    • Hatch doors
    • Hardtops
    • Radar arches
    • Swimming platforms
    • Interior liners
    • Moldings
    • ABS-PC-ACRYLIC-PVC-PC
    • Interior trims
    • Interior fittings
  • Industrial-Architectural:
    • FRP 2 part tanks/baffles
    • Pipes, ducts, control boxes
    • FRP cooling towers
    • Building fascia’s
    • Signage, windows and doors
    • Composites bridges/walkways
    • Composite utility poles
    • Communication towers
    • Wind power blades
    • Nacelle’s
    • Communication buildings
    • Amusement park
    • Pultrusions-platforms

Information provided by Engineered Bonding Solutions, LLC (EBS)

Vendors:
Available Properties
  • Viscosity, B
  • Viscosity, A
  • Tensile Strength
  • Elongation at Break, Postcured
  • Adhesive Bond Strength, ASTM D1002, Single Lap Shear vs. Al 6061
  • Cure Time, Fixture Time
  • Working Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.