MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Special Metals INCONEL® Alloy X-750
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: A nickel-chromium alloy similar to INCONEL alloy 600 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good resistance to corrosion and oxidation along with high tensile and creep-rupture properties at temperatures to about 1300°F (700°C). Its excellent relaxation resistance is useful for high-temperature springs and bolts. Used in gas turbines, rocket engines, nuclear reactors, pressure vessels, tooling, and aircraft structures. Standard product forms are round, flats, extruded section, forging stock, plate, sheet, strip, pipe, tube, and wire.

Data provided by the manufacturer, Special Metals.

Key Words: MIL-N-7786, MIL-N-8550, MIL-S-23192, MIL-N-24114; NACE MR-01-75; AFNOR NC 15 FeT, SAE AMS 5542, 5582, 5583, 5598, 5667 - 5671, 5698, 5699, 5747, 7246, UNS N07750; BS HR505; ASTM B 637; ASME SB-637, Boiler Code Section III; Werkstoff Nr. 2.4669
Vendors:
Available Properties
  • Density
  • Tensile Strength, Ultimate, Precipitation Hardened prior to test
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield, Precipitation Hardened. Value at room temperature
  • Tensile Strength, Yield, Precipitation Hardened prior to test
  • Elongation at Break, Precipitation Hardened
  • Elongation at Break, Precipitation Hardened prior to test.
  • Rupture Strength
  • Rupture Strength
  • Rupture Strength
  • Rupture Strength
  • Rupture Strength
  • Electrical Resistivity
  • Magnetic Permeability, at 200 Oersted (15.9 kA/m)
  • Curie Temperature
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Aluminum, Al
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co
  • Copper, Cu
  • Iron, Fe
  • Manganese, Mn
  • Nickel, Ni, Including Cobalt
  • Niobium, Nb (Columbium, Cb), Includes Ta
  • Silicon, Si
  • Sulfur, S
  • Titanium, Ti
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Special Metals (includes the former Inco Alloys International Inc.)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.